RAW MATERIALS
 
Typical Characteristics

Property
Test Method
Unit Typical Value
Melt Flow Index (190oC/5.0 kg.) ASTM 1238 gm./10 min. 1.0
Density 23oc ASTM D 1505 GM./cm3 0.9555
Tensile Strength at Yield ASTM dD 638 kg./cm3 22.5
Elongation At Break % ASTM D 638 % 15
Flexuval Modulus ASTM D 790 kg./cm 28.200
Notched Izod Impact Strength ASTM D 256 kg./cm no break
Vicat Softening Point ASTM D 1525oc 127
Note : Based on injection moulded 3.2 mm thickness type one specimen of ASTM D 638
 
KNITTING
 
 
The filament is knitted to fabric form by knitting machines. We are producing fabric 100 mess/sq. inch to 250 mess/sq.inch. Knitting is done by quality High-Tech Flat Raschel Machines.
 
EXTURDER
 
 
The raw material that is used to produce the filament in this extrusion process is HDPE granules. Filament can be made in variable colors and with minimum of 80 dinear to maximum of 300 dinear sizes.
 
WINDING
 
 
The hank form filament is then winded into small bobbins.
 
WARPING
 
 
Here, the filament is loaded to the beam for the knitting.
 
PACKING
 
 
REELING
 
 
The conversion of the filament to hank form is done in this reeling process.
 
 
 